WORLDWIDE
Thermally Conductive Compounds
- Item No. : ThermPass 1203
- Porduct Name : Thermally Conductive Polymer
Our company has been specializing in manufacturing Thermally Conductive Polymer for many years, offering Plastic Heat Sink and Thermally Conductive Compound with superior quality.
ThermPass 1203 is polypropylene-based, thermally conducting, electrically insulating and flame-retardant injection grade. ThermPass 1203 is a non-halogenated, non-phosphate thermally conductive compound for LED Heat Sink (Plastic Heat Sink , Insulation Heat Sink) application.ThermPass 1203 is in compliance with IEC 62560, IEC 60695 and IEC 60968.
ThermPass 1203 is polypropylene-based, thermally conducting, electrically insulating and flame-retardant injection grade. ThermPass 1203 is a non-halogenated, non-phosphate thermally conductive compound for LED Heat Sink (Plastic Heat Sink , Insulation Heat Sink) application.ThermPass 1203 is in compliance with IEC 62560, IEC 60695 and IEC 60968.
Feature :
1. Good thermal conductivity
2. UL94 1.5mm V-0
3. Good processability for injection molding
4. Design freedom & stylish colors
2. UL94 1.5mm V-0
3. Good processability for injection molding
4. Design freedom & stylish colors
Application :
Plastic Heat Sink , Insulation Heat Sink
Specification :
PROPERTIES | STANDARD |
VALUE |
UNIT |
PHYSICAL | |||
Color | white and colored |
||
Melt Flow Rate, 200°C/10 kg | ASTM D1238 |
14 |
g/10min |
Elongation at break (MD/TD) | ASTM D792 |
2.2 |
g/cm3 |
MECHANICAL | |||
Tensile Strength, 50 mm/min | ASTM D638 |
125 |
Kg/cm2 |
Flexural Strength | ASTM D790 |
300 |
Kg/cm2 |
Flexural Modulus | ASTM D790 |
63100 |
Kg/cm2 |
Impact Strength, 1/8" Notched | ASTM D256 |
20 |
J/m |
THERMAL | |||
Thermal conductivity | ISO 22007-2 |
1.6 |
W/m-K |
HDT, 0.45 MPa, unannealed | ASTM D648 |
130 |
oC |
ELECTRICAL | |||
Surface resistivity | ASTM D257 |
>1E+12 |
Ohm/sq |
Mold shrinkage | ASTM D955 |
0.006 |
cm/cm |
FLAME CHARACTERISTICS | |||
UL94 V-0 Flammability Rating | pass |
1.5 |
mm |
Processing parameters | VALUE |
UNIT |
Pre-drying condition | ||
Drying Temperature | 80 - 100 |
oC |
Drying Time | 2 - 4 |
hours |
Injection molding condition | ||
Injection Temperature | 190-210 |
oC |
Injection Pressure | Medium |
|
Injection Speed | Medium - Fast |
|
Mold Temperature | 50 |
oC |