Permanently Anti-static Film for aluminum bags
KennFilm 1601 is a permanently antistatic PE/PA film for aluminum lamination, with surface resistivity below…
Product detailsMoisture barrier and antistatic packaging materials for electronic component protection.

KennFilm 1601 is a permanently antistatic PE/PA film for aluminum lamination, with surface resistivity below…
Product details
KennFilm 1605 is a permanently antistatic PE film for ESD zipper bags, with surface resistivity below…
Product details
KennFilm 1681 is a permanently antistatic aluminum laminated bag material with high oxygen and water barrier…
Product details
KennFilm 5100 is a permanently antistatic multi-layer co-extruded PE/nylon surface protective film with…
Product details
KF-1410 clear dissipative tubing is a multilayer PE blown film with surface resistivity below 10¹¹ Ω/sq…
Product detailsNo matching content.
This is a multi-layer material designed for electrostatic and moisture protection in ESD and moisture barrier packaging.
Its structure, composed of polyester, aluminum foil, polyamide, and polyethylene, is engineered to meet the requirements of a wide range of applications.
Feature:| Kenner Film Series |
Physical Properties | Surface Resistivity | Interior ESD Shelf Life Years |
Static Shielding nJ |
MVTR g/m2.day |
||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Film Thickness (mm) |
Length (mm) |
Width (mm) |
Seal Width (mm) |
Base Polymer | Tensile Strength (MD/TD) Kgf/15mm |
Tear Strength (MD/TD) Kgf |
Heat Seal Strength Kgf/15mm |
Puncture Strength (MD/TD) Kgf |
Exterior side 50% RH Ω/sq |
Interior side 12%/50% RH Ω/sq |
|||||||
| Test Method | Thickness Gauge |
ASTM D-882 | ASTM D-882 | ASTM D-882 | FTMS 101C 2065.1 |
ANSI/ESD STM11.11 |
ANSI/ESD STM11.11 |
Kenner Method | ANSI/ ESD STM11.31 |
ASTM F-1249 |
|||||||
|
Kenner Film Series
KF-6583
|
Physical Properties |
Film Thickness (mm)
0.135
Test Method: Thickness Gauge
|
Length (mm)
250
|
Width (mm)
250
|
Seal Width (mm)
10
|
Base Polymer
PET/ AL/ PA/ PE
|
Tensile Strength (MD/TD) Kgf/15mm
4.5 / 1.5
Test Method: ASTM D-882
|
Tear Strength (MD/TD) Kgf
> 1.3 / 1.8
Test Method: ASTM D-882
|
Heat Seal Strength Kgf/15mm
> 4
Test Method: ASTM D-882
|
Puncture Strength (MD/TD) Kgf
6
Test Method: FTMS 101C 2065.1
|
Surface Resistivity |
Exterior side 50% RH Ω/sq
< 9E10
Test Method: ANSI/ESD STM11.11
|
Interior side 12%/50% RH Ω/sq
< 9E10
Test Method: ANSI/ESD STM11.11
|
Other Properties |
Interior ESD Shelf Life Years
> 5
Test Method: Kenner Method
|
Static Shielding nJ
< 20
Test Method: ANSI/ ESD STM11.31
|
MVTR g/m2.day
< 0.005
Test Method: ASTM F-1249
|
|
Kenner Film Series
KF-6583
|
Physical Properties |
Film Thickness (mm)
0.135
Test Method: Thickness Gauge
|
Length (mm)
482.6
|
Width (mm)
406.4
|
Seal Width (mm)
10
|
Base Polymer
PET/ AL/ PA/ PE
|
Tensile Strength (MD/TD) Kgf/15mm
4.5 / 1.5
Test Method: ASTM D-882
|
Tear Strength (MD/TD) Kgf
> 1.3 / 1.8
Test Method: ASTM D-882
|
Heat Seal Strength Kgf/15mm
> 4
Test Method: ASTM D-882
|
Puncture Strength (MD/TD) Kgf
6
Test Method: FTMS 101C 2065.1
|
Surface Resistivity |
Exterior side 50% RH Ω/sq
< 9E10
Test Method: ANSI/ESD STM11.11
|
Interior side 12%/50% RH Ω/sq
< 9E10
Test Method: ANSI/ESD STM11.11
|
Other Properties |
Interior ESD Shelf Life Years
> 5
Test Method: Kenner Method
|
Static Shielding nJ
< 20
Test Method: ANSI/ ESD STM11.31
|
MVTR g/m2.day
< 0.005
Test Method: ASTM F-1249
|

From material selection to customized support, our team is ready to help with dependable solutions for advanced manufacturing.